Corrosion has always been the number one factor affecting the life of aluminum plates. Although the aluminum plate processed through a certain process can be used in a complex environment, because there are many factors that cause corrosion of the aluminum plate, no perfect processing process can guarantee that the aluminum plate will not corrode. There are three main reasons for the corrosion of aluminum plates: environmental factors, metallurgical factors and stress factors, which affect each other.
1. Environmental factors
The environmental factors that affect stress corrosion of aluminum plates are: ion species, ion concentration, solution pH, oxygen and other gases, corrosion inhibitors, ambient temperature, ambient pressure, and so on.
The stress corrosion conditions of 2A12 and 7A04 aluminum plates in different atmospheric environments were studied. It was found that aluminum plates have different sensitivity to stress corrosion in different environments and are more sensitive in marine environments. The marine environment contains a large amount of salt, and Cl- will pass through the maintenance film on the outer surface of the aluminum plate and enter the interior, causing corrosion.
The experiment indicates that when the mass concentration of HNO3 solution is between 20% and 40%, the corrosion of aluminum plate is intensified, and the corrosion rate of aluminum plate reaches the highest point when the concentration is about 35%. In concentrated HNO3 solution, the stress corrosion of the aluminum plate is not obvious. The reason for this phenomenon is that a dense oxide film is formed on the surface of the aluminum plate, which prevents further corrosion of HNO3.
2. Metallurgical factors
The metallurgical factors mainly include the influence of casting method, processing method and hot stress corrosion on gold. It is found that the cathodic polarization increases the sensitivity of stress corrosion of aluminum plate, and the stress corrosion sensitivity of friction stir welding is lower than that of welding.
It is generally believed that properly treated 6061-T6 and 3004 aluminum plates will not corrode. Different metallurgical factors change the type of the outer film of the aluminum plate, and cause the internal structure of the aluminum plate and the change of the crystal structure, which affects the electrochemical behavior and mechanical behavior of the aluminum plate, resulting in different sensitivity to stress corrosion of the aluminum plate.
3. Stress factors
The stress factors mainly include load type, load size, loading direction, and loading speed. In terms of corrosion, the direction of stress must be perpendicular to the grain boundaries in order to be able to separate them. One of the key factors for stress corrosion to occur is stress. Different stress effects will produce different effects. Corrosion fatigue caused by the interaction of alternating stress and the environment is usually significantly different from stress corrosion cracking caused by fixed stress. Corrosion fatigue usually has more severe consequences than stress corrosion. In addition, the difference in loading speed will also affect the sensitivity of the aluminum plate to stress corrosion.
The above three factors often affect each other. Even if the simple processing procedure can protect the aluminum plate from the influence of one kind of environmental corrosion, it is difficult to avoid the corrosion of the other two kinds of environments. Therefore, it is necessary to comprehensively consider the use environment of the aluminum plate and do a good job of anti-corrosion.