Reasons for the brittleness of aluminum plates
With the continuous development of my country’s economy, the market’s demand for aluminum sheets is increasing. Many manufacturers see this business opportunity and turn to aluminum sheets. However, due to poor technology and inexperience in production, these aluminum sheet manufacturers often produce aluminum sheets. All have the phenomenon of brittleness, so what causes this situation? Next, I will give you a brief introduction.
1. For performance degradation caused by poor confluence of diversion ribs, the length of the ribs and the outer surface, the confluence of the ribs and the ribs should be appropriately increased, or the compression ratio should be increased, and the pressure of the die can be changed by changing the length of the straight section of the die. To adjust the flow resistance; in the mold design stage, you can choose different compression ratios to change the extrusion pressure, but you must pay attention to the compression ratio of the die head to be compatible with the compression ratio of the extruder screw; you can also adjust the extrusion by changing the formula Process parameters, increase the perforated plate to change the size of the melt pressure.
2. The cooling rate of the shaping mold and the temperature of the cooling water often do not attract enough attention. The role of the cooling water is to cool and shape the stretched macromolecular chains in time to achieve the purpose of use.
3. The design of the die section is unreasonable, especially the distribution of internal ribs and the treatment of the angle of the interface, which will cause stress concentration. It is necessary to improve the design and eliminate the right and acute angles at the interface.
4. Uneven output from the die, resulting in inconsistent profile wall thickness or inconsistent density. This also caused the difference in the mechanical properties between the two sides of the profile. As for the thin wall and other non-standard profiles, I won't say more here.
5. The pressure of the die is insufficient. The pressure at the die is directly determined by the compression ratio of the die, especially the length of the straight section of the die. If the compression ratio of the die is too small or the straight section is too short, the aluminum plate product will not be dense, which will affect the physical properties.