The most demanding aluminum foil coil quality and extrusion aluminum foil process

Aug 12, 2021

Leave a message

The most demanding aluminum foil coil quality and extrusion aluminum foil process

 

  The quality requirements of aluminum foil coils are as follows:

    (1) The thickness of the two stacked aluminum foils should be uniform, and the thickness deviation should not exceed ±3%.

    (2) Spray double oil evenly on the double surface before unwinding, and trim 10-15 mm on each side after unwinding. If the double oil spray is uneven, the dark side will have color difference after rolling. The edge trimming is to cut the edge cracks, and at the same time to ensure the same width of the two double rolled aluminum foils.

    (3) There should be no wrinkles or folds during winding. The tension of the two aluminum foils should be the same as possible, the tension is generally 10-20MPa, to avoid the existence of these defects when one is loose and the other is tight. It is easy to cause rolling breakage.

    (4) The cutting edge should be free of cracks, burrs, and edges.

    (5) For the aluminum foil that is separately rolled up, the end surface should be neat and free of layering, and the coiling tension should be controlled reasonably. Avoid loose coiling or "ribbing".

    (6) The original state of the two aluminum coils to be combined should be similar to each other. If intermediate recovery annealing is to be carried out, annealing should be carried out after double bonding. Otherwise, due to the difference in the original state, the rolling deformation is not uniform during the double rolling, and it is easy to cause the strip to break.

  Extruded aluminum foil process

  1. When using high-density tooth extrusion aluminum mold to try out the mold, the aluminum support must be a short aluminum rod or pure aluminum rod of 150-200mm.

  2. Before trying the mold, the center of the aluminum extruder, the extrusion shaft, the ingot barrel, and the outlet of the mold base must be adjusted to a straight line.

  3. During the trial and production process, the temperature of the aluminum rod should be kept between 480-520℃.

  4. The heating of aluminum materials should be heated according to the conventional temperature, the temperature is controlled at about 480℃, the diameter is less than 200mm, and the temperature needs to be maintained for not less than 2 hours. If the split mold is used, the heat preservation should be more than 3 hours; During the production process, if the mold with a diameter of more than 200mm is kept for 4-6 hours, it can ensure that the core and the outside of the mold can be evenly heated.

  5. Before mold trial or production, cylinder cleaning gasket must be used to clean the inner container of the ingot barrel and check whether the extruder is operating normally.

  6. During the trial production process, the automatic gear of the extruder needs to be turned off, and the switches need to be reset. Start the pressure slowly from the minimum pressure, and the discharge time is about 3-5 minutes. We must control the pressure during the aluminum filling process. The pressure is controlled within 100Kg/cm2, the current is controlled within 2-3A, and the material can be discharged at 80-120Kg/cm2, and then it can be appropriately accelerated, when the normal pressure is less than 120Kg/cm2.

  7. In the production process, if there is a phenomenon such as mold blockage, partial teeth, too large speed deviation, etc., stop immediately, and unload the mold in a point-retract mode, so as to avoid mold scrap.