Factors that cause 5052 aluminum plate to fail to produce qualified
Patterned aluminum plates are widely used. Three-reinforced, five-reinforced, and pointer-type patterned aluminum plates are all common varieties. You can see patterned aluminum plates in construction, transportation, decoration, and refrigeration equipment.
1. The unqualified mechanical properties of the annealed sheet are generally caused by the annealing temperature being too low or the holding time too short; or because the heat treatment can strengthen the cooling rate of the aluminum alloy sheet after annealing.
2. The unqualified mechanical properties of annealed semi-hard products are generally caused by low annealing temperature, short holding time, perhaps too high annealing temperature, too long holding time, etc.
3. The unqualified mechanical properties of the quenched aging plate are generally due to the low quenching heating temperature or short holding time; perhaps the cooling rate during quenching is too slow. If the quenching heating temperature is too high and the material is severely overburned, its mechanical properties can also be significantly reduced.
In order to obtain the plates with qualified mechanical properties, it is necessary to strictly implement the heat treatment process regulations, and to grasp and check the working conditions of the heat treatment furnace and the temperature measurement surface in time. For artificially aged panels, if over-aging occurs, if the instantaneous temperature is too high or the aging time is too long, the strength of the material will also decrease.